Applications
Applying fiberglass mesh on the wall during construction can solve the problems of wall crack, ripple, rot and efflorescence and also has the effects of thermal insulation, sound insulation and insect prevention.
Grade A/B/C/D comparison of fiberglass mesh
Fiberglass mesh can be made into mesh with different specifications and effects according to different engineering needs, and its hardness mainly depends on mesh surface coating, also called alkali-resistant glue, which can be classified into urine glue and emulsion. Among them, the emulsion is classified into soft glue, medium soft glue and hard glue. The urine glue-coated mesh is hard, brittle and easy to break. The emulsion-coated mesh has good toughness and is not easy to break. The mesh suitable for some construction sites must be well-shaped and soft, so soft glue should be used. If you need to use a tough mesh, hard glue is preferred. Hard glue can be easily applied on the wall and does not prick your hands during construction. No matter which fiberglass mesh is applied on the wall, it should be alkali-resistant, so customers can buy with confidence.
Specification | Weight | Mesh(mesh/inch) | Model of Raw Yarn | Fiber Diameter | Resin Content | Fracture Strength | Surface Treatment | ||||
Warp | Weft | Warp | Weft | Warp | Weft | Warp | Weft | ||||
75g 5*5 | 75±5 | 5±0.5 | 5±0.5 | 67 | 250 | 11 | 13 | 13±2 | 900 | 1200 | Lotion |
110g 5*5 | 110±5 | 5±0.5 | 5±0.5 | 97*2 | 282 | 11 | 13 | 18±2 | 1300 | 1700 | Lotion |
145g 5*5 | 145±5 | 5±0.5 | 5±0.5 | 130*2 | 375 | 11 | 13 | 15±2 | 1500 | 2100 | Lotion |
180g 4*4 | 180±5 | 4±0.5 | 4±0.5 | 160*2 | 315 | 11 | 13 | 14.5±2 | 1600 | 2900 | Lotion |